It is generally preferred in degreasing operations of parts such as pots, pans or aluminum profiles that are processed in aluminum presses. Also suitable for copper and zinc. The bath is installed at a concentration of 3-5% by weight, the processing time is 5-10 minutes, the temperature 60 – 80 ° C will be sufficient for surface cleaning.