It is a zinc phosphate product which is applied to increase the corrosion resistance of iron and steel parts in electrostatic powder coating applications. Single component, provides 2-5 g / m2 coating, working temperature 60-70 ° C degree, processing time should be between 5-10 minutes. There is no need to use activation. Creates a homogeneous and compact coating. The application has a sludge-forming structure, so the phosphate sludge should be cleaned at regular intervals, measurements should be made and water and PHORIC ZDN should be added on.